Polyimide Film (HN)
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Polyimide
Film is produced by cast method, which has high temperature resistance,
resistance to
|
|
|
radiation
and excellent dielectric properties. It is applicable to electrical
insulating of the class H electric
|
|
motor
and other electrical equipments, and other use electrical insulating
materials.
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
1. Thickness and Tolerance:
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Thickness(um)
|
12.5
|
20
|
25
|
30
|
40
|
50
|
75
|
100
|
125
|
150
|
175
|
200
|
225
|
250
|
Tolerance(um)
|
+1
|
+2
|
+2
|
+2
|
+2
|
+2
|
+3
|
+4
|
+4
|
+6
|
+6
|
+6
|
+6
|
+6
|
-1
|
-1
|
-1
|
-1
|
-2
|
-2
|
-3
|
-3
|
-4
|
-6
|
-6
|
-6
|
-6
|
-6
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
2. Properties:
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Number
|
Item
|
Unit
|
Index
|
25um
|
40um
|
50um
|
75um
|
100um
|
125um
|
150um
|
175um
|
200um
|
225um
|
1
|
Density
|
Kg/m³
|
1425±10
|
2
|
Tensile Strength (MD & TD)
|
Mpa
|
≥185
|
≥165
|
≥110
|
3
|
Elongation (MD & TD)
|
%
|
≥60
|
4
|
Shrinkage (MD &
TD)
|
%
|
≤1.0 (150oC)
|
≤3.0 (400oC)
|
5
|
Electric Strength
(breakdown)
|
v/um
|
≥240
|
≥200
|
≥180
|
≥160
|
≥150
|
≥110
|
48Hz~62Hz
|
6
|
Surface Resistance,200oC
|
Ω
|
≥1.0x1013
|
7
|
Volume Resistance,200oC
|
Ω.M
|
≥1.0x1010
|
8
|
Dielectric
Constant 48Hz~62Hz
|
-
|
3.5±0.4
|
9
|
Dielectric
Loss Factor 48Hz~62Hz
|
-
|
≤4.0x103
|